Sapphire

Sapphire

“Deep” titanium-diffused preform sliced open andn polished to reveal the depth of color penetration. Note that much of the color layer will be removed during polishing. Despite claims by manufacturers, the so-called “deep diffusion” process showed no more color penetration than that claimed in the original Linde patents, i.e. up to 0.50 mm.

Image number
LGI-001641
Enhancements
Heat + Diffusion of external coloring agents (H-D)
Lighting conditions
Diffuse Light Field (Transmitted Light)
Photographer
E. Billie Hughes
Field of view
Not recorded

Reference(s)